Aluminium and aluminium alloys · Сплав AW-2007 - 3.1645

Aluminum alloy AW-2007 (3.1645): technical specifications and applications

Technical parameters of the AW-2007 aluminum alloy

StandardApplication fieldAlternative designations
EN 573-3: defines the requirements for the chemical composition and classification of wrought aluminum alloys.Manufacturing of high-strength components by forging and machining, intended for use in loaded engineering assemblies and critical structures.European
EN 573-3: defines the requirements for the chemical composition and classification of wrought aluminum alloys.Manufacturing of high-strength components by forging and machining, intended for use in loaded engineering assemblies and critical structures.AlCu4PbMgMn, 3.1645

Chemical composition of AW-2007 alloy (mass fraction, %)

Si<0,8
Fe<0,8
Cu3,3-4,6
Mn0,5-1,0
Mg0,4-1,8
Cr<0,1
Ni<0,2
Zn<0,2
Other elements<0,5
AlBase

Mechanical properties of AW-2007 material

Material conditionThickness, mmTensile strength (Rm), MPaYield strength (Rp0,2), N/mm²Elongation (A50 mm), %Brinell hardness, HB (max.)Modulus of elasticity, MPaCoefficient of thermal expansion, μm/m-°CThermal conductivity, W/mKElectrical resistivity, Ωmm²/m
Material conditionThickness, mmTensile strength (Rm), MPaYield strength (Rp0,2), N/mm²Elongation (A50 mm), %Brinell hardness, HB (max.)Modulus of elasticity, MPaCoefficient of thermal expansion, μm/m-°CThermal conductivity, W/mKElectrical resistivity, Ωmm²/m
T330-804002501010071 00023,61340,051
T330-804002501010071 00023,61340,051
T4<80390260910571 00023,61340,051

Physical parameters

The density of the AW-2007 aluminum alloy is 2.82 kg/dm³. The material demonstrates excellent machinability on high-speed CNC machines and has increased fatigue strength, making it an optimal choice for precision mechanical engineering from EV Group China.

International equivalents of AW-2007 alloy

USA (ASTM)Germany (DIN)Japan (JIS)Russian equivalents (GOST)
ANSI AA2007AlCuMgPbA1050AMg3